Teryl® - Cetaver® mixed cord
Construction :
- Made of :
- BRAID = Continuous Polyester yarn.
- CORE = Discontinuous Glass yarn (Verranne).
We realised a mixed cord with an outer braid in polyester to decrease the itching problems caused by glass.
- To be impregnated by the users.
- Can be heat stabilized on request (1 hour at 190 °C) .
- The letter T is added to the reference . This stabilization is recommended for diameters up to 16 mm. It eliminates a part of the textile ensimage.
PRE-PREG : On request, we can make a stage B impregnation with a class F resin. They are heat stabilized prior to impregnation.
- The % of resin is ≥ 50% for diameters < 10 mm and ≥ 60% for diamaters ≥ 10 mm of the weight of the cord.
- They are presented cut at length and packed in a waterproof aluminised bag and must be stored in a cool place (life time 6 months).
Heat resistance : Class F 155°C.
Applications :
- ELECTROTECHNICAL INDUSTRY.
Used mainly as stuffing and filling of sections and parts with impregnation by the user.
Producto | Diameter | Weight per meter | Unit | selección |
---|---|---|---|---|
TV 01 | 5 mm | 14 g/m | M | |
TV 02 | 7 mm | 22 g/m | M | |
TV 03 | 9 mm | 33 g/m | M | |
TV 04 | 11 mm | 43 g/m | M | |
TV 05 | 13 mm | 65 g/m | M | |
TV 06 | 16 mm | 66 g/m | M | |
TV 07 | 18 mm | 110 g/m | M | |
TV 08 | 20 mm | 132 g/m | M | |
TV 10 | 25 mm | 183 g/m | M | |
TV 11 | 30 mm | 281 g/m | M | |
TV 12 | 35 mm | 335 g/m | M | |
TV 13 | 40 mm | 380 g/m | M | |
TV 14 | 45 mm | 493 g/m | M | |
TV 15 | 50 mm | 530 g/m | M | |
TV 17 | 60 mm | 700 g/m | M |